TIMETAL® 829 (Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si) Titanium Alloy
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy
Material Notes: Titanium content above is calculated as the remainder and may not reflect the actual range. Weldable, High Strength, High Temperature, Creep Resistant Alloy Features: TIMETAL 829 combines creep resistance up to 540°C with good oxidation resistance. It is weldable and like TIMETAL 685, TIMETAL 829 has good forgeability. It is nonmagnetic. Typical heat treatment for this alloy: Solution heat treat: 1050°C for 30 mins, air cool. Aging heat treatment: 625°C for 2 hours, air cool. Data provided by TIMET.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Notched Tensile Strength
- Fatigue Strength
- Fracture Toughness
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|