TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Solution Treated; 0.025 - 1.000 in Sheet and Plate; Per ASTM B265)

 

Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy

Key Words: Titanium 6-4 ELI; UNS R56401

Material Notes:
Titanium content above is calculated as the remainder and may not reflect the actual range.

Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are spcific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.

Features: A lower strength version of TIMETAL 6-4 with improved toughness, cryogenic ductility, and SCC resistance. Major uses are in the medical implant field, marine structural components, and oil and gas production. This variant is available for fracture critical applications. This alloy is available in most common product forms including billet, bar, wire, plate, and sheet.

Data provided by TIMET.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Bend Radius, Minimum
  • Electrical Resistivity
  • Magnetic Permeability
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Melting Point
  • Liquidus
  • Maximum Service Temperature, Air
  • Beta Transus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。