|   TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136)  Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy Key Words: Titanium 6-4 ELI; UNS R56401 Material Notes: Titanium content above is calculated as the remainder and may not reflect the actual range.
 Medium To High Strength General-Purpose Alloy.   Minimum tensile property data below are spcific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb. Features: A lower strength version of TIMETAL 6-4 with improved toughness, cryogenic ductility, and SCC resistance. Major uses are in the medical implant field, marine structural components, and oil and gas production.  This variant is available for fracture critical applications.  This alloy is available in most common product forms including billet, bar, wire, plate, and sheet.  Data provided by TIMET. 
| | 
    | Available Properties |  
    | DensityTensile Strength, UltimateTensile Strength, YieldElongation at BreakReduction of AreaModulus of ElasticityPoissons RatioShear ModulusBend Radius, MinimumElectrical ResistivityMagnetic PermeabilityCTE, linear 20°CCTE, linear 250°CCTE, linear 500°CSpecific Heat CapacityMelting PointLiquidusMaximum Service Temperature, AirBeta Transus
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |