Latrobe CBS-50™ NiL VIM-VAR High Performance Carburizing Bearing and Gear Steel
Subcategory: High Carbon Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: CBS-50 NiL VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. The chemistry is engineered such that when suitably carburized and heat treated the case will have a microstructure of fine tempered martensite with an even distribution of fine carbides. The primary advantage of CBS-50 NiL VIM-VAR steel over conventional through hardening M50 is the relatively high fracture toughness properties of the core. Because the alloy can be carburized, surface stresses can be controlled to provide excellent rolling contact fatigue characteristics.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Density
- Critical Temperature
- Modulus of Elasticity
- Charpy Impact
- CTE, linear 20°C
- CTE, linear 500°C
- Transformation Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|