Latrobe CBS-600™ VIM-VAR Carburizing Bearing and Gear Steel
Subcategory: High Carbon Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe impact and fracture toughness characteristics.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Density
- Critical Temperature
- Hardness, Rockwell C
- Ultimate Tensile Strength
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Reduction of Area
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- CTE, linear 20°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|