Latrobe Lescalloy® 16NCD13 VAC-ARC High Strength Alloy Steel
Subcategory: Low Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: 16NCD13 VAC-ARC is a premium quality low alloy, carburizing casehardenable vacuum arc remelted steel which takes its name from the French industry designation. In the carburized condition, its high case hardness is combined with desirable impact and fracture toughness characteristic in the core. Additionally, superior cleanliness makes Lescalloy 16NCD13 VAC-ARC steel ideally suited for critical aerospace gear and actuator applications.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Hardness, Rockwell C
- Ultimate Tensile Strength
- Tensile Strength, Yield
- Elongation at Break
- Charpy Impact
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|