Latrobe Lescalloy® AF 1410 VIM-VAR; 6 in High Strength Alloy Steel
Subcategory: High Carbon Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical, fracture-sensitive aerospace structural applications. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide superior
cleanliness, ingot homogeneity, and to enhance mechanical properties.Heat Treatment - 857°C - 1 hour oil quench; -73°C - 1 hr air warm; 510°C - 5 hrs air cool Information Provided by Timken Latrobe Steel.
| Available Properties |
- Density
- Critical Temperature
- Ultimate Tensile Strength
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Charpy Impact
- Fracture Toughness
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|