Latrobe Lescalloy® UT-18 VAC-ARC; 6 in. round High Strength Alloy Steel
Subcategory: Low Alloy Steel; Medium Carbon Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting is employed to provide a preferred ingot solidification and superior microcleanlinessInformation Provided by Timken Latrobe Steel.
| Available Properties |
- Ultimate Tensile Strength
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Izod Impact Notched
|
|
|
|
| Property Data |