Latrobe Tatmo-VN™ ASTM M7 High Speed Steel
Subcategory: Tool Steel; High Carbon Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: TATMO-VN is an M7 type high speed steel modified by alloy balancing and a nitrogen addition to develop superior hardness response in heat treatment. It is an excellent grade for
many cutting tool applications that require an optimum balance of red hardness, edge toughness and wear resistance. The combination of outstanding properties and high
hardness response makes Tatmo-VN a logical alternative for cobalt high speed steels in may cutting tool applications. Typical applications for Tatmo-VN high speed steel include twist drills, taps, end mills, reamers and milling cutters.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Specific Gravity
- Density
- Critical Temperature
- Hardness, Rockwell C
- Modulus of Elasticity
- Izod Impact Unnotched
- Machinability
- CTE, linear 20°C
- CTE, linear 500°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|