Latrobe DuraTech™ T15 Powder Metal High Speed Steel (ASTM T15)
Subcategory: Tool Steel; High Carbon Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: DuraTech T15 powder metallurgy high speed steel is cobalt-bearing super high speed steel which can be heat treated to a hardness as high as 67 Rockwell C. A high volume of hard vanadium carbides provides very high wear resistance. The cobalt content provides excellent resistance to softening at high service temperatures (red or hot hardness). These properties translate into extended retention of hard, sharp cutting edges on tools produced from DuraTech T15. Because of the powder metal (PM) manufacturing, DuraTech T15 is far easier to grind and exhibits impact toughness that is more than double that of traditional, ingot-cast T15 high speed steel. Typical tooling applications in which DuraTech T15 excels include high-performance
broaches, form tools, milling cutters, end mills, taps, and reamers. DuraTech T15 is the high speed steel of choice for any cutting application on strong or abrasive materials that generate high cutting tool temperatures.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Specific Gravity
- Density
- Critical Temperature
- Hardness, Rockwell C
- Modulus of Elasticity
- Machinability
- CTE, linear 20°C
- CTE, linear 500°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|