Latrobe LSS™ H11 Hot Work Tool Steel (ASTM H11)
Subcategory: Tool Steel; Hot Work Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides for the higher toughness, with some reduction in wear resistance and temper resistance. TLS H11 hot work tool steel is a deep-hardening, air-hardening steel that exhibits minimal size change during heat treatment. It has good resistance to thermal fatigue cracking (heat checking) and excellent resistance to gross cracking and thermal shock when water cooled in service. TLS H11 hot work tool steel is recommended for hot tooling applications where maximum resistance to cracking is required. Such applications include hot punches, die
casting dies, forging dies, hot shear blades, hot gripper dies, and extrusion tooling.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Specific Gravity
- Density
- Critical Temperature
- Hardness, Rockwell C
- Modulus of Elasticity
- Charpy Impact
- Machinability
- CTE, linear 20°C
- CTE, linear 500°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|