Latrobe LSS™ H13 PQ Hot Work Tool Steel
Subcategory: Tool Steel; Hot Work Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications. TLS H13 PQ is melted using an electric-arc furnace, is refined by the argon-oxygen-decarburization (AOD) process, and is further enhanced to aerospace quality levels using Vacuum-Arc or Electro-Slag Remelting. These special melting practices along with special thermo-mechanical and annealing treatments result in ultra-high microcleanliness and a homogeneous, fine-grained microstructure.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Specific Gravity
- Density
- Critical Temperature
- Hardness, Rockwell C
- Modulus of Elasticity
- Charpy Impact
- Machinability
- CTE, linear 20°C
- CTE, linear 500°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|