Latrobe Magnadie - RF Modified Premium H-13 Hot Work Die Steel
Subcategory: Hot Work Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: Magnadie-RF is a premium quality 5% chromium hot work die steel. The chemistry of Magnadie-RF steel is a modification of the premium quality H-13 chemistry. Magnadie-RF steel is designed for increased production rates and increased tool life. Though the chemistry is unique, Magnadie-RF steel meets the selective standards of the North American Die Casting Association, as well as other industrial specifications including Chrysler`s specification for die casting applications.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Density
- Hardness, Rockwell C
- Ultimate Tensile Strength
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Machinability
- CTE, linear 20°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|