Latrobe LSS™ H21 Hot Work Tool Steel (ASTM H21)

 

Subcategory: Tool Steel; Hot Work Steel; Alloy Steel; Metal

Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Material Notes:
TLS H21 hot work tool steel is a low-carbon, tungsten hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is intended for elevated-temperature service in which tool operate at dull-red heat. For best results, TLS H21 hot work steel should not be water cooled in service unless the tool design includes a continuous flow of internal water cooling. Spray cooling and thermal shock should be avoided. Tools should be thoroughly preheated before entering service. TLS H21 hot work tool steel is recommended for difficult hot work tooling applications such as brass extrusion tooling, brass die casting dies, hot punches, and forging die inserts.

Information Provided by Timken Latrobe Steel.

Available Properties
  • Specific Gravity
  • Density
  • Critical Temperature
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • Charpy Impact
  • Machinability
  • CTE, linear 20°C
  • CTE, linear 500°C
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。