Latrobe LSS™ P20 Mold Steel (ASTM P20)
Subcategory: Medium Carbon Steel; Alloy Steel; Mold Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: TLS P20 mold steel is a versatile, low-alloy tool steel that is characterized by good toughness at moderate strength levels. The steel is commonly used for plastic injection mold cavities and tooling and for die casting dies for zinc. TLS P20 is typically sold in the prehardened condition at a hardness of approximately 300 HBW.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Specific Gravity
- Density
- Critical Temperature
- Hardness, Rockwell C
- Modulus of Elasticity
- Machinability
- CTE, linear 20°C
- CTE, linear 500°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|