Latrobe LSS™ A9 Tool Steel (ASTM A9)
Subcategory: Tool Steel; Cold Work Steel; Hot Work Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: TLS A9 tool steel is a 5% chromium tool steel with a unique combination of properties which make it suitable for both cold work and hot work tooling applications. The combination of nickel, vanadium, and a relatively low carbon content provide excellent toughness and hardenability with good wear resistance. Typical applications for TLS A9 tool steel include shear blades, punches and dies, forming tools, hot upsetting dies, and hot gripper dies.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Specific Gravity
- Density
- Hardness, Rockwell C
- Modulus of Elasticity
- Machinability
- CTE, linear 20°C
- CTE, linear 500°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|