Latrobe Graph-Air® Cold Work Tool Steel (ASTM A10)
Subcategory: Tool Steel; Cold Work Steel; High Carbon Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: Graph-Air tool steel is an air-hardening, graphitic tool steel with outstanding resistance to metal-to-metal sliding wear and galling. The steel contains a uniform dispersion of graphite particles which impart excellent machinability and non-seizing characteristics. The graphite particles make the steel self-lubricating in dry environments, and help to retain oil in lubricated environments. Graph-Air tool steel can be hardened to over 60 Rockwell C from a relatively low hardening temperature, which minimizes size change and distortion during heat treatment.
Typical applications include thread gauges, master gages, cams, bushings, sleeves, meat granulator plates, arbors, forming rolls, shear blades, punches, dies, bar feed guides and other machine tool parts.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Specific Gravity
- Density
- Hardness, Rockwell C
- Modulus of Elasticity
- Izod Impact Unnotched
- Machinability
- CTE, linear 20°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|