Latrobe LSS™ D5 Tool Steel (ASTM D5)
Subcategory: Tool Steel; Air-Hardening Steel; High Carbon Steel; Alloy Steel; Metal
Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Material Notes: TLS D5 tool steel is an air hardening, high-carbon, high-chromium, tool steel that is characterized by a cobalt addition which provides unique resistance to galling and pick-up. The cobalt also imparts some resistance to tempering, which makes TLS D5 suitable for some semi-hot work tooling applications.Information Provided by Timken Latrobe Steel.
| Available Properties |
- Specific Gravity
- Density
- Critical Temperature
- Hardness, Rockwell C
- Modulus of Elasticity
- Izod Impact Unnotched
- Machinability
- CTE, linear 20°C
- CTE, linear 500°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|