|   Latrobe DuraTech™ 20CV Powder Metal Stainless Tool Steel  Subcategory: Tool Steel; Stainless Steel; High Carbon Steel; Alloy Steel; Metal Close Analogs: Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co. Material Notes: DuraTech 20CV is a highly wear resistant, powder metallurgy stainless tool steel.  The steel containes a large volume of extremely hard vanadium carbides, wich provide excellent wear resistance.  DuraTech 20CV contains the highest amount of chromium of any high-vanadium stainless steel currently available.  The chromium-rich matrix provides outstanding corrosion resistance.  DuraTech 20CV is a versatile stainless tool steel with a unique combination of high wear resistance, high corrosion resistance, good impact toughness, and excellent polishability.  This combination of properties is the result of the fine grain size, small carbides, and superior cleanliness of the powder metallurgy (PM) microstructure.  DuraTech 20CV excels in applications, which require a combination of high wear resisatance.  The unique combinations of properties makes DuraTech 20CV an excellent steel for plastic injection feed screws, barrel liners, screw tips, and mold cavities, especially for plastic resins which contain abrasive fill
 
| | 
    | Available Properties |  
    | DensityHardness, Rockwell CModulus of ElasticityMachinabilityCTE, linear 20°CCTE, linear 500°C
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |