Domex® 390XP Extra High-strength Cold-forming Steel
Subcategory: Low Alloy Steel; Metal
Material Notes: Extra High-strength Cold-forming Steel, HSLA Characteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex® high strength steels offers a number of benefits compared to ordinary structural steels: Lower weight, Simpler production, Lower creep rate, Longer useful life, Higher load-bearing capacity, Lower transport costs, Reduced stocks, Lower overall cost. Iron content is approximate - exact value is not reported by the manufacturer. Data provided by SSAB Tunnplat.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bend Radius, Minimum
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|