Docol® DC04 (Fe P04) Deep-drawing Steel
Subcategory: Carbon Steel; Low Carbon Steel; Metal
Material Notes: Deep-drawing Steel Comments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported by the manufacturer. Data provided by SSAB Tunnplat.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |