Docol® 1000 DP High-strength Steel
Subcategory: Low Alloy Steel; Metal
Material Notes: High-strength Steel Characteristics: The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel is heated to 200-400°C and then acquires its final structure to which the steel owes it toughness and good formability. This unique annealing procedure produces a tempered martensitic structure that accounts for the high strength of the steel. Both annealing and tempering are carried out in an inert atmosphere to prevent the steel from oxidizing, and the steel strip runs through a pickling bath between quenching and tempering, in order to remove the thin oxide film formed in the quenching process. Comments: Docol - Cold Rolled Steel - Ultra high-strength steel (UHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content calculated as remainder. Applications: Tubes, Transport cages, Child seats for cars, Truck load stays, Venetian blinds, Washers, Hose clips, Clutch plates, Hedge cutters, Springs, Spades, Safes, Knives, Train seats, Ladders, Circlips, Saw blades, Chains, Bumpers, Bicycles, Containers, Clips Data provided by SSAB Tunnplat.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bend Radius, Minimum
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|