Dogal F30 Metal-coated Mild Steel
Subcategory: Carbon Steel; Low Carbon Steel; Metal
Material Notes: Metal-coated Mild Steel Comments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufacturer. Data provided by SSAB Tunnplat.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bend Radius, Minimum
|
|
|
|