Universal Wire Works 309L Stainless Steel Electrode
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Key Words: AWS E309L-15,16
Material Notes: Iron content is calculated as remainder. Universal 309L is the same as E309 with the exception of the carbon content. The lower carbon content permits this alloy when used in corrosive environments where it is necessary to protect against intergranular corrosion due to carbide precipitation without the use of stabilizers such as titanium or columbium. The deposited weld metal is not as strong in elevated temperatures as the standard 309 or the stabilized alloys. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Tensile Strength, Ultimate
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|