Universal Wire Works 320 Stainless Steel Electrode
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Key Words: AWS E320-15,16
Material Notes: Iron content is calculated as remainder. Universal 320 produces a fully austenitic deposit for welding Carpenter Stainless No. 20Cb-3 (wrought form) or Durimet 20 (cast form) or similar alloys. The 320 alloy was developed to give improved resistance to the corrosive action of sulfuric acid. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Tensile Strength, Ultimate
- Elongation at Break
|
|
|
|
| Property Data |