Universal Wire Works ER308H Stainless Steel Bare Wire
Subcategory: Stainless Steel; Metal
Material Notes: Iron content is calculated as remainder. This filler metal is the same as ER308, except that the allowable carbon content has been restricted to the higher portion of the 308 range. Carbon content in the range of 0.04-0.08 provides higher strength. ER308H is used for welding 304H base metal. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|