Universal Wire Works ER310 Stainless Steel Bare Wire
Subcategory: Stainless Steel; Metal
Material Notes: Iron content is calculated as remainder. This alloy is used for welding 310 base metal, stainless steel to mild steel, welding 304 clad steels, and stainless steel overlay work. Information provided by Universal Wire Works for their line of welding wire and filler metal.