Universal Wire Works ER316LSi Stainless Steel Bare Wire
Subcategory: Stainless Steel; Metal
Material Notes: Iron content is calculated as remainder. This filler metal is the same as the 316L, except for the silicon content. The additional silicon improves the washing and wetting behavior of the weld metal. This feature reduces the finishing costs of welds particularly on thin base metals. Information provided by Universal Wire Works for their line of welding wire and filler metal.