Universal Wire Works ER420 Stainless Steel Bare Wire
Subcategory: Stainless Steel; Metal
Material Notes: Iron content is calculated as remainder. This alloy is the same as ER410, except for the carbon content. By incorporating a higher carbon 420 becomes an excellent surfacing alloy for applications requiring corrosion and abrasion resistance. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |