Material Notes: Iron content is calculated as remainder. This alloy contains 4 to 6 percent chromium and about 0.50 percent molybdenum. It is used for welding base metals of similar composition, usually pipe or tubing. This alloy is air hardening and requires preheating and postweld heat treatment. Information provided by Universal Wire Works for their line of welding wire and filler metal.