Universal Wire Works ER630 Stainless Steel Bare Wire
Subcategory: Stainless Steel; Metal
Material Notes: Iron content is calculated as remainder. This alloy is designed primarily for welding ASTM A564 Type 630, 17 percent chromium, 4 percent nickel, and precipitation-hardening stainless steel. The composition is modified to eliminate the present of ferrite stringers in the martensitic micro-structure, which has a damaging effect on mechanical properties. Dependent on the weld size, the weld metal may be used in the as welded, welded-plus precipitation-hardened, or welded-plus-solution-treated-plus-precipitation-hardened. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|