Universal Wire Works 82 Nickel Alloy Welding Wire
Subcategory: Nickel Alloy; Nonferrous Metal
Key Words: AWS A5.14 Class ERNiCr-3; ASME SFA-5.14 Class ERNiCr-3
Material Notes: Alloy 82 is used for TIG, MIG and submerged-arc welding of Inconel type alloys 600 and 601, Incoloy type alloy 800 and welding the clad side of steel clad with nickel chromium alloy. Dissimilar metals welding applications include: joining stainless steels to carbon steel, Nickel 200, Monel type 400; Inconel and Incoloy type alloys to stainless steels, carbon steel, Nickel 200 and Monel type 400. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Tensile Strength, Ultimate
- Elongation at Break
|
|
|
|