Universal Wire Works A Nickel Alloy Welding Wire
Subcategory: Nickel Alloy; Nonferrous Metal
Key Words: AWS A5.11 Class ENiCrFe-2; ASME SFA-5.11 Class ENiCrFe-2
Material Notes: Alloy A is used for arc welding various dissimilar combinations of austenitic and ferritic steels and high nickel alloys. For example, when welding Inconel and Incoloy type alloys to carbon steel, stainless steel, Nickel 200, Monel type alloys, and nickel alloys, it is the product of choice. Alloy A is used to weld Monel type alloys, Nickel 200, and carbon steel to stainless steels. Alloy A is recommended for welding Incoloy type alloy 800 and 9% nickel steel to themselves. Electrode sizes 3/32 and 3/16 diameter can be used in all positions, while the larger 5/32 and 3/16 diameter are normally used in the flat or horizontal positions. POWER SUPPLY DCRP. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Tensile Strength, Ultimate
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|