Universal Wire Works 70S-2 Steel Welding Wire
Subcategory: Carbon Steel; Metal
Key Words: AWS A5.18 Class ER70S-2
Material Notes: Iron content is calculated as remainder. Universal 70S-2 is designed for TIG or MIG welding of all carbon steels. The tensile strength exceeds the base metal on single pass deposits on gaged carbon steel. Alloy 70S-2 is triple deoxidized using zirconium, titanium, and aluminum in addition to magnesium and silicon deoxidizers. Alloy 70S-2 is excellent for X-ray quality welds on carbon steels with CO2 or Argon/CO2 gas mixtures as the shielding gas. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|