Universal Wire Works 80SD-2 Steel Welding Wire

 

Subcategory: Carbon Steel; Metal

Key Words: AWS A5.28 Class ER80S-D2

Material Notes:
Iron content is calculated as remainder.

Universal 80SD-2 is a manganese, molybdenum, silicon low alloy steel wire producing weld deposits of unusually high strength, ductility and impact properties. This alloy was developed for the welding of medium carbon and sulphur bearing free machining steels. When MIG welding use CO2 shielding gas. The amounts of manganese and silicon in this alloy provide good salvaging action in the weld pool resulting in sound, porosity-free weld.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Available Properties
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Charpy Impact, Notched Low Temp
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。