Universal Wire Works 90SB-3L Steel Welding Wire
Subcategory: Carbon Steel; Metal
Key Words: AWS A5.28 Class ER90SB-3L
Material Notes: Iron content is calculated as remainder. The 90SB-3L alloy is the same as the 90SB-3 alloy with the exception of a restricted carbon content. Universal 90SB-3 is a 2.25% chromium and 1% molybdenum alloy for welding on steel of similar composition. This alloy is designed for joints in process piping systems, boilers, or pressure vessels. Weld deposits require preheat and postweld heat treatments for optimum mechanical properties. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |