Universal Wire Works EB-2 Steel Welding Wire
Subcategory: Carbon Steel; Metal
Key Words: AWS A5.23 Class EB-2; ASME SFA-5.23 Class EB-2
Material Notes: Iron content is calculated as remainder. Universal EB-2 is a 1.25% chromium 0.5% molybdenum alloy designed for submerged-arc welding of base metals of similar composition. Deposits have high strength and excellent creep resistance. Applications include large diameter pipe and pressure vessels. Preheat, interpass temperature and postweld heat treatments are required for optimum mechanical properties. Mechanical properties depend upon various welding variables such as the flux used, the preheat and interpass temperature, the heat input and postweld heat treatment. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|