Universal Wire Works Alloy 5056 (AMS 4182) Aluminum Alloy Filler Metal
Subcategory: Aluminum Alloy; Nonferrous Metal; AISI 5000 Series Steel; Metal
Material Notes: Aluminum content is calculated as remainder. Primarily used to inert-gas-arc weld base metals of similar composition requiring joints with strength, corrosion and heat resistance comparable to those of the base metal. Information provided by Universal Wire Works for their line of welding wire and filler metal.