Universal Wire Works Alloy 4043 (AMS 4190) Aluminum Alloy Filler Metal
Subcategory: Aluminum Alloy; Nonferrous Metal; AISI 4000 Series Steel; Metal
Material Notes: Aluminum content is calculated as remainder. Alloy 4043 is a 5% silicon aluminum alloy designed to weld many similar and dissimilar cast and wrought aluminum parts. This alloy is excellent for types 4043, 6063, 5052, 6061, 355, 356 and others. Extensively used with the gas tungsten arc and gas metal arc processes with Argon shielding gas. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|