Universal Wire Works Alloy 2319 (AMS 4191) Aluminum Alloy Filler Metal
Subcategory: Aluminum Alloy; Nonferrous Metal
Material Notes: Aluminum content is calculated as remainder. Alloy 2319 is used on applications requiring good strength at high temperatures (600°F) and many cryogenic and aircraft parts. Primarily used where weld joints are capable of being heat treated to high strength. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|