Universal Wire Works Alloy AZ92A (AMS 4395) Magnesium Alloy Filler Metal
Subcategory: Magnesium Alloy; Nonferrous Metal
Material Notes: Magnesium content is calculated as remainder. Magnesium alloy AZ92A is primarily used as an inert gas arc filler metal for welding magnesium alloys of similar composition, particularly where consistently high quality joints are mandatory. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|