Universal Wire Works Alloy BNi-1A (AMS 4776) Nickel Base Brazing Filler Metal
Subcategory: Nickel Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes: Low Carbon (compare to BNi-1) Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|