Universal Wire Works 6Al-4V (ELI) (AMS 4956) Titanium Alloy Filler Metal
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Material Notes: Titanium content is calculated as remainder. Universal titanium alloy 6Al-4V (ELI) is similar to type 6Al-4V in chemical analysis with the exception of Extra Low Interstitial gases (ELI). By controlling these contaminating gases the fracture toughness is greatly increased. Alloy 4956 is used to weld liquid hydrogen tankage and airframe parts requiring a high fracture toughness. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |