Universal Wire Works Inconel 600 (AMS 5687) Nickel Alloy Filler Metal
Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal; Nickel Base
Material Notes: Alloy 600 is recommended when good oxidation and corrosion resistance at elevated temperatures are required. This alloy is used extensively in aircraft engines and primarily in exhaust equipment. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|