Universal Wire Works Inconel 69 (AMS 5778) Filler Metal
Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal; Nickel Base
Material Notes: Inconel Filler Metal 69 is used for gas tungsten arc and gas metal arc welding of Inconel Alloy 722 and Inconel x-750. Typical applications for filler metal 69 include gas turbine and aircraft parts such as turbine blades, vanes, discs and springs. Age hardening info: 1950°F/2 hr.,A.C. + 1300°F/20 hr.,A.C. Information provided by Universal Wire Works for their line of welding wire and filler metal.