Universal Wire Works Stellite 31 (AMS 5789) Filler Metal
Subcategory: Superalloy; Nonferrous Metal; Cobalt Alloy; Cobalt Base
Material Notes: Cobalt content is calculated as remainder. Haynes Stellite Alloy No. 31 is a cobalt base alloy having very good stress-rupture endurance and creep strength properties. No. 31 can be welded with the gas tungsten arc, gas metal arc and plasma welding processes. Information provided by Universal Wire Works for their line of welding wire and filler metal.