Universal Wire Works Haynes 188 (AMS 5801) Filler Metal
Subcategory: Superalloy; Nonferrous Metal; Cobalt Alloy; Cobalt Base
Material Notes: Cobalt content is calculated as remainder. Haynes Alloy No. 188 is often used with the gas tungsten arc and gas metal arc processes. Alloy 188 has excellent high temperature strength and oxidation resistance to 2100°F combined with post aging ductility. Small additions of lanthanum account for the excellent oxidation resistance. This alloy has been successfully used for gas turbine, airframe, chemical and nuclear applications. More specifically, the alloy can be used to weld transition ducts, spray bars, flame holders, liners in jet engines and combustion cans. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|