Universal Wire Works Alloy A286VM (AMS 5805) Filler Metal
Subcategory: Superalloy; Stainless Steel; Iron Base; Metal
Material Notes: Iron content is calculated as remainder. The same alloy as A286, with the exception of being vacuum melted. Primarily used to inert-gas-arc weld base metals of similar composition requiring joints with strength, corrosion and heat resistance comparable to those of the base metal. Information provided by Universal Wire Works for their line of welding wire and filler metal.