Universal Wire Works 17-7 (AMS 5824) Filler Metal
Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal
Material Notes: Iron content is calculated as remainder. Universal 17-7PH is a precipitation-hardening filler metal designed for gas tungsten arc and gas metal arc welding of precipitation-hardening, corrosion resistant steels of similar composition where the weld area is required to have comparable strength and corrosion resistance to those of parent metal. Information provided by Universal Wire Works for their line of welding wire and filler metal.