Universal Wire Works Inconel 625 (AMS 5837) Filler Metal
Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal; Nickel Base
Material Notes: Inconel Filler Metal 625 is recommended for gas metal arc and gas tungsten arc welding of nickel base alloys 625 and 601, Incoloy alloys, carbon steels, low alloy steels and stainless steels. This alloy is useful for jet engine applications requiring excellent stress-rupture strength, oxidation resistance to 1200°F, plus outstanding fatigue strength and cryogenic properties. Many engine applications include ducting systems, combustion systems, thrust reverser assemblies, fuel nozzles, afterburner parts and spray bars. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|